Guide Content
Operational framework for procurement execution
System Boundary and Scope Definition
PC basket molds operate within defined material and thermal windows: melt 280–320°C, mold temperature 80–120°C, shrinkage compensation 0.5–0.7% across wall thickness 1.5–4 mm. Supplier scorecard scope encompasses cavity geometry, gate location, cooling circuit design, and surface finish (optical grade ≤0.8 µm Ra for transparent baskets). Define boundary between mold supplier responsibility (cavity accuracy ±0.05 mm, draft angles 0.5–1° for PC's poor flow), OEM design engineering (wall thickness optimization, rib placement), and production control (melt temp hold, dwell pressure). Exclude post-mold finishing (annealing, coating) from mold qualification but flag annealing requirements in scorecard commentary to prevent thermal stress cracking in PC's amorphous structure.
Interface Rules and Data Dependencies
Scorecard data flows: (1) Design handoff—OEM provides CAD with PC-specific wall analysis (1.5–3 mm nominal), gate diameter 2–4 mm, cooling line spacing ≤50 mm; mold supplier returns shrinkage simulation and thermal FEA. (2) Tooling approval—supplier submits first-article mold inspection (FAMI) report with cavity dimensional data, gate balance verification, and cooling uniformity maps; OEM validates against optical clarity spec and dimensional stack. (3) Process window—supplier establishes melt viscosity curve (PC: 280–320°C range), dwell pressure schedule, and cooling time (typically 20–40 sec for 2 mm wall); OEM confirms cycle time and part quality targets. (4) Production feedback—defect traceability (sink marks, warping, gate witness) linked to mold condition and process parameter drift; scorecard updated quarterly.
Process Robustness and Change Control
PC's poor mold flow (low fluidity at 280–320°C) demands tight gate design and cavity pressure monitoring. Scorecard robustness criteria: cavity pressure uniformity ±5%, mold temperature stability ±3°C, gate freeze-off time <2 sec to prevent gate blush. Change control protocol: any mold cavity modification (polishing, EDM repair, cooling line rework) requires re-qualification via 50-part production trial and optical clarity re-validation. PC's chemical sensitivity (poor solvent resistance) mandates mold cleanliness audits—residual release agent or coolant contamination causes haze and dimensional drift. Establish SPC limits on shrinkage (0.5–0.7% ±0.05%) and warpage (<0.3 mm for typical basket geometry); if exceeded, trigger mold inspection and cavity pressure re-mapping before production restart.
Qualification Plan and Go/No-Go Gates
PC basket mold qualification phases: (1) Design review—validate PC material spec (1.20 g/cm³ density, 2.3 GPa flexural modulus), confirm wall thickness 1.5–4 mm and cooling strategy for uniform shrinkage. Gate 1: Thermal FEA sign-off and shrinkage simulation (±0.05% tolerance). (2) First article—produce 100 parts at melt 300°C ±5°C, mold 100°C ±5°C; measure dimensions, optical clarity (haze <2%), and gate witness. Gate 2: 95% parts within spec, zero sink marks or flow lines. (3) Process capability—run 500-part trial across mold cavity; calculate Cpk ≥1.33 for critical dimensions and shrinkage. Gate 3: Sustained Cpk, no defects attributable to mold design. (4) Production handoff—supplier provides mold maintenance schedule, cavity pressure baseline, and coolant specification; OEM confirms SPC charting and defect escalation protocol.
Commercial Controls and SLA Design
PC basket mold SLA framework: (1) Availability—mold uptime ≥98% (target <2% downtime for maintenance/repair); supplier compensates OEM at 1.5× daily production loss if downtime exceeds 4 hours unplanned. (2) Dimensional hold—cavity dimensions maintain ±0.05 mm over 50,000 parts; if drift detected, supplier performs polishing at no cost. (3) Quality gate—defect rate <0.5% (PC-specific: haze, warpage, gate witness); supplier absorbs scrap and rework cost if root cause is mold design or maintenance. (4) Responsiveness—mold modification requests (gate balance, cooling adjustment) completed within 10 working days; emergency changes within 48 hours. (5) Escalation—supplier provides monthly SPC reports, cavity pressure logs, and preventive maintenance records; quarterly business reviews track scorecard metrics (on-time delivery, quality consistency, cost-per-cavity-hour).
Operating Model and Continuous Improvement
Establish joint governance: OEM assigns mold engineer and quality lead; supplier designates cavity owner and process engineer. Monthly cadence: (1) Defect triage—classify PC-specific failures (sink marks from slow cooling, gate blush from residual moisture, haze from contamination); assign root cause (mold design, maintenance, process drift). (2) SPC review—validate shrinkage 0.5–0.7% and dimensional trends; if Cpk slides below 1.33, trigger preventive mold inspection. (3) Cooling optimization—analyze thermal imaging data; adjust coolant flow or line routing if temperature uniformity drifts >3°C. (4) Supplier scorecard—track on-time mold delivery, first-pass quality rate, and cost-per-cavity-hour; cascade results to supplier incentive plan. Annual strategy: benchmark PC mold performance against industry (target: <0.3% defect rate, >99% availability); evaluate cavity design refresh if shrinkage compensation cannot achieve ±0.05% tolerance.