Decision Context and Winning Criteria
Choosing between ABS (Acrylonitrile Butadiene Styrene) and PE (Polyethylene) for chair mold in high-volume consumer products requires systematic comparison across mechanical properties, processing characteristics, and total cost of ownership. ABS processes at 220β260Β°C with 0.4β0.7% shrinkage; PE requires 180β230Β°C with 2.0β3.0% shrinkage. For 3.0β5.0 mm wall targets, this shrinkage difference directly affects tooling design and dimensional control. ABS offers tight dimensional tolerance from low shrinkage, while PE provides excellent chemical resistance across pH range. The decision framework must weight surface finish and cycle time for cost-per-part economics against tooling investment and long-term part cost.